4.7 Article

Tensile properties of friction stir welded joints of 2024 aluminum alloys in different heat-treated-state

Journal

MATERIALS & DESIGN
Volume 30, Issue 6, Pages 2211-2221

Publisher

ELSEVIER SCI LTD
DOI: 10.1016/j.matdes.2008.08.034

Keywords

Heat treatments; Welding; Mechanical

Ask authors/readers for more resources

In this study, the different heat-treated-state 2024 Al-alloys were friction stir welded. The tensile properties of the joints have a tendency to increase with the precipitation hardening of the base material. The peak tensile properties have been obtained in the T6 (100 degrees C - 10 h) joint. It is observed that the weld zone is strengthened by the friction stir welding process for the 2024-0 joint. The fracture regions are detected near the nugget for W joint, the interface between the nugget and the thermomechanically affected zone for T4 and T6 joints and base material for O joint. (C) 2008 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available