4.7 Article

Effect of TiO2 addition on grain shape and grain coarsening behavior in 95Na1/2Bi1/2TiO3-5BaTiO3

Journal

JOURNAL OF THE EUROPEAN CERAMIC SOCIETY
Volume 31, Issue 10, Pages 1915-1920

Publisher

ELSEVIER SCI LTD
DOI: 10.1016/j.jeurceramsoc.2011.04.002

Keywords

Grain growth; Interface; Perovskite; Microstructure-final; Lead-free piezoelectric

Funding

  1. Ministry of Knowledge Economy (MKE), Republic of Korea [PM007-10-01-01]
  2. Ministry of Education, Science and Technology [2009-0094039]
  3. Korea Evaluation Institute of Industrial Technology (KEIT) [PM007-10-01] Funding Source: Korea Institute of Science & Technology Information (KISTI), National Science & Technology Information Service (NTIS)

Ask authors/readers for more resources

Grain coarsening behavior in the 95Na(1/2)Bi(1/2)TiO(3)-5BaTiO(3) system has been studied as a function of the addition of TiO2. As the amount of added TiO2 was increased, the grain shape changed to a more faceted cube, indicating an increase in the step free energy of the facets, and hence a rise in the critical driving force for appreciable growth of grains. Grain coarsening behavior also changed from pseudo-normal to abnormal with an increasing TiO2 concentration and thus increased faceting. The pseudo-normal behavior observed in the system without TiO2 addition also changed to quite abnormal behavior during extended sintering. These observations support our theoretical prediction based on the coupling effects between the maximum driving force for growth and the critical driving force for appreciable growth. (C) 2011 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available