4.7 Article

Effect of electrolysis condition of zinc powder production on zinc-silver oxide battery operation

Journal

ENERGY CONVERSION AND MANAGEMENT
Volume 52, Issue 4, Pages 1876-1880

Publisher

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.enconman.2010.11.001

Keywords

Electrolytic zinc powder; Morphology; Specific surface; Zinc-silver battery; Discharge time

Ask authors/readers for more resources

A research conducted to produce zinc powder through electrolysis of alkaline solutions by using various concentrations of KOH and zincate in the bath. Different current densities were applied for each concentration and then, morphological changes of Zn powder batches were examined by scanning electron microscopy. Afterward, an anode electrode was produced from each pack of powder. Thirty-six Zn-AgO battery cells were prepared totally. Discharge parameters of the cells were examined and time-voltage curves were analyzed. Discharge times were investigated for various conditions of Zn deposition and the proper terms were suggested. It has been seen that increase of KOH concentration and decrease of zincate ion in the bath solution will change the zinc morphology and increase the resultant battery discharge time. The longest time of discharge, before reduction of cell voltage to 1.25 V. was 7.91 min. This result was obtained for Zn powder produced in zincate concentration of 0.5 M, KOH concentration of 11 M and current density of 2500 A/m(2). (C) 2010 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available