4.0 Article

Tuning the Crystallization Temperature of Amorphous Ge2Sb2Te5 by O and Si Recoil Implantation

Journal

ELECTROCHEMICAL AND SOLID STATE LETTERS
Volume 14, Issue 3, Pages H124-H127

Publisher

ELECTROCHEMICAL SOC INC
DOI: 10.1149/1.3527941

Keywords

-

Funding

  1. MIUR

Ask authors/readers for more resources

The amorphous to crystal transition temperature has been measured in capped (10 nm SiO2) and uncapped Ge2Sb2Te5 (GST) films (20 nm thick) after irradiation with a 40 keV Ge+ in the range between 5 x 10(13) and 1 x 10(15) ions/cm(2). In the capped samples the crystallization temperature increases with fluence (15 degrees C at 1 x 10(15) ions/cm(2)). This effect is due to the doping of the GST layer with a few atom percent of recoiled O and Si atoms. The influence of the chemical species on the crystallization kinetics overcomes the effect of the ion-induced local rearrangement that instead decreases the transition temperature by a few degrees in the uncapped samples. Recoil implantation through the use of a thin capping layer may then be a viable alternative to the direct doping of chalcogenide thin films. (C) 2010 The Electrochemical Society. [DOI: 10.1149/1.3527941] All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.0
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available