Accelerated corrosion of five commercial steels under a ZnCl2–KCl deposit in a reducing environment typical of waste gasification at 673–773K

Title
Accelerated corrosion of five commercial steels under a ZnCl2–KCl deposit in a reducing environment typical of waste gasification at 673–773K
Authors
Keywords
-
Journal
CORROSION SCIENCE
Volume 50, Issue 7, Pages 1900-1906
Publisher
Elsevier BV
Online
2008-05-04
DOI
10.1016/j.corsci.2008.03.004