Effects of sintering temperature and initial compaction load on alpha-alumina membrane support quality

Journal

CERAMICS INTERNATIONAL
Volume 40, Issue 7, Pages 11299-11309

Publisher

ELSEVIER SCI LTD
DOI: 10.1016/j.ceramint.2014.03.134

Keywords

Sintering; alpha-alumina; Compaction load; Pore size

Funding

  1. Council of Scientific and Industrial Research (CSIR), New Delhi, Government of India [22(0630)/13/EMR-II]

Ask authors/readers for more resources

This work reports the effect of sintering temperature and compaction load on the quality of a-alumina (similar to particle size < 1 mu m) membrane support for dry compaction method. We analyzed the membrane synthesis process to get good quality membrane support in a more economical way by reducing the holding time (4 h) at different sintering temperatures. The effect of initial compaction load on porosity, pore size, flexural strength and shrinkage during synthesis of alpha-alumina support at various sintering temperatures was investigated. It was found that at 1500 degrees C sintering temperature and 350 IN compaction load, the support exhibited least porosity of similar to 1.4% and least pore sizes of 67 rim, whereas at 1200 degrees C and 50 kN compaction load, the support showed the highest porosity of similar to 55% and highest pore size of similar to 505 nm.Maximum flexural strength of similar to 200 MPa was obtained for the support synthesized at 1500 degrees C sintering temperature and 350 kN load. (C) 2014 Elsevier Ltd and Techna Group S.r.l. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available