4.7 Article

The effect of prolonged milling time on comminution of quartz

Journal

POWDER TECHNOLOGY
Volume 330, Issue -, Pages 266-274

Publisher

ELSEVIER SCIENCE BV
DOI: 10.1016/j.powtec.2018.02.033

Keywords

Quartz; Conventional ball milling; Prolonged grinding; Size distribution; Morphology; Microstructure

Funding

  1. Industrial Technology Institute of Sri Lanka [TG 16/127]

Ask authors/readers for more resources

The effect of prolonged milling on quartz has been investigated by conventional ball milling. The milling efficiency was enhanced by a proper selection of grinding media (alumina), ball containing fraction, initial particle size and amount of quartz being ground. The milling was carried out in 72 h cycles (total milling time 360 h) under constant operational mill speed of 130 rpm. The effect of milling time on particle size, morphology, purity, and microstructure of quartz was examined. Results indicate that particle size reduced by >96%. It is also found that lattice strain and dislocation density increased while crystallite size decreased substantially as a function of milling time. The change in particle shape from elongated flake to spherical along with relative size determine the shape of particle size distribution curve, uniformity of lattice strain and extent of alumina contamination. The alumina contamination reported for longest milling duration is <3.3% and insignificant during the early stage of milling. The prolonged milling effects on particle size, morphology, purity, and microstructure of quartz enormously under applied milling conditions. (C) 2018 Elsevier B.V. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available