Sintering effects of mullite-doping on mechanical properties of bovine hydroxyapatite

Publisher

ELSEVIER SCIENCE BV
DOI: 10.1016/j.msec.2017.03.290

Keywords

Sintering; Mechanical properties; Bovine derived hydroxyapatite; Mullite

Ask authors/readers for more resources

In this study, sintering effects on microstructural behavior of bovine derived hydroxyapatite doped with powder mullite are considered in the temperature range between 1000 C-omicron and 1300 C-omicron. Results show that maximum values of both compressive strength and microhardness are achieved in the samples sintered at 1200 C-omicron for all mullite additions of 5, 7.5, 10 and 12.5 wt. Moreover, above 1000 C-omicron, decomposition of HA and new phase formations such as whitlockite and gehlenite play a major role in both compressive strength and microhardness properties which increase up to 10 wt mullite reinforcement. (C) 2017 Elsevier B.V. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.3
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available