Effect of mineral components on sintering of ash particles at low temperature fouling conditions

Journal

FUEL PROCESSING TECHNOLOGY
Volume 141, Issue -, Pages 82-92

Publisher

ELSEVIER SCIENCE BV
DOI: 10.1016/j.fuproc.2015.06.004

Keywords

Sintering; Gasification; Mineral mapping; Dilatometer; Shrinkage

Funding

  1. project of Development of the Design Technology of a Korean 300 MW Class IGCC Demonstration Plant - Korea Institute of Energy Technology Evaluation and Planning (KETEP)
  2. Ministry of Trade, Industry & Energy of the Korean government [2011951010001B]
  3. Korea Evaluation Institute of Industrial Technology (KEIT) [2011951010001B] Funding Source: Korea Institute of Science & Technology Information (KISTI), National Science & Technology Information Service (NTIS)

Ask authors/readers for more resources

The ash deposition phenomenon in the coal gasification process is a severe problem for continuous operation. The ash deposition rate is influenced by the behavior of ash particles on the deposit target. Dropped coal ash particles, which exhibit different behaviors on the deposit surface such as attachment, rebounding, and removal, were observed through the view port of a drop tube furnace (DTF). The different behaviors may be influenced by the state of the ash particles such as the sintering phenomenon, which is a function of the mineral content. To verify the mineral components important in sintering among the ash particles, transformation of the particle shape of synthetic ash reacted at 900 degrees C was analyzed through a scanning electron microscope (SEM). The Fe, Ca, and Mg components were the main factors for sintering and agglomeration. The Fe, Ca, and Mg components sintered with Si and Al were observed in the mineral mapping of deposited coal ash by scanning electron microscopy with energy dispersive X-ray spectroscopy (SEM-EDX) analysis. Sintering characteristics of coal ash were analyzed by the dilatometer technique. Sintering temperature,shrinkage, and sintering activation energy (E-sin) were all found to be related to the Fe, Ca, and Mg contents. (C) 2015 Elsevier B.V. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available