Hot corrosion behavior of Al 2 O 3 –Cr 2 O 3 refractory by molten glass at 1200 °C under static condition

Title
Hot corrosion behavior of Al 2 O 3 –Cr 2 O 3 refractory by molten glass at 1200 °C under static condition
Authors
Keywords
A. Ceramic, A. Glass, B. SEM, B. XRD, C. High temperature corrosion
Journal
CORROSION SCIENCE
Volume 102, Issue -, Pages 153-160