4.4 Article

Porous Silicon Fabrication and Surface Cracking Behavior Research Based on Anodic Electrochemical Etching

Journal

FUEL CELLS
Volume 21, Issue 1, Pages 52-57

Publisher

WILEY-V C H VERLAG GMBH
DOI: 10.1002/fuce.202000048

Keywords

Crack Behavior; Drying Process; Electrochemical Etching; Nanostructure; Porous Silicon

Funding

  1. National Natural Science Foundation of China [61764009, 51904134, 51504117, 51974143, 51762043]
  2. National Key RAMP
  3. D Program of China [2018YFC1901801, 2018YFC1901805]
  4. Major Science and Technology Projects in Yunnan Province [2019ZE007]
  5. Key Project of Yunnan Province Natural Science Fund [2018FA027]
  6. Yunnan Youth Fund Project [2016FD037]
  7. Program for Innovative Research Team in University of Ministry of Education of China [IRT_17R48]

Ask authors/readers for more resources

The study systematically examined the relationship between preparation conditions, nanostructure, and cracking behavior of PSi surface. It was found that the preparation conditions and nanostructure influenced the cracking behavior, while the extent of cracking was controlled by the porosity of the material.
Porous silicon (PSi) was fabricated based on anodic electrochemical etching, and the relationship between preparation conditions, nanostructure and PSi surface crack behavior were systematically studied. The effects of silicon wafer resistivity (doping concentration), etching time, and etching current density on nanostructure of PSi were investigated. Results indicated that lower resistivity was beneficial to etching process and led to higher porosity with uniform nano-channels, and surface crack was more intense during drying process. Thickness and porosity of the porous layer are both initially increased and then decreased with increasing etching time. Direction of capillary stress depended on pore geometry, which further affected crack shape (shrinkage or crimp) of surface layer of PSi. Cracking extent was controlled by porosity, that the surface cracking layer began to peel off when the porosity exceeded 70%. Finally, a geometry and porosity-controlled model was proposed to describe the cracking behaviors of PSi surface layer.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.4
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available