4.7 Article

Bioelectrochemical treatment and recovery of copper from distillery waste effluents using power and voltage control strategies

Journal

JOURNAL OF HAZARDOUS MATERIALS
Volume 371, Issue -, Pages 18-26

Publisher

ELSEVIER
DOI: 10.1016/j.jhazmat.2019.02.100

Keywords

Bioelectrochemical system; Copper recovery; Distillery waste; MPPT; Applied 0.5v

Funding

  1. Natural Environment Research Council (NERC), United Kingdom [NE/L014106/1, NE/L014203/1]
  2. Resource Recovery from Waste (RRfW) Programme, United Kingdom
  3. BBSRC, United Kingdom [BB/L013711/1, BB/R010412/1]
  4. FLEXIS research project, United Kingdom [WEFO 80835]
  5. BBSRC [BB/R010412/1] Funding Source: UKRI
  6. EPSRC [EP/N009746/1] Funding Source: UKRI
  7. NERC [NE/L014203/1, NE/L014246/1, NE/L01422X/1] Funding Source: UKRI

Ask authors/readers for more resources

Copper recovery from distillery effluent was studied in a scalable bioelectro-chemical system with approx. 6.8 L total volume. Two control strategies based on the control of power with maximum power point tracking (MPPT) and the application of 0.5 V using an external power supply were used to investigate the resultant modified electroplating characteristics. The reactor system was constructed from two electrically separated, but hydraulically connected cells, to which the MPPT and 0.5 V control strategies were applied. Three experiments were carried out using a relatively high copper concentration i.e. 1000 mg/L followed by a lower concentration i.e. 50 mg/L, with operational run times defined to meet the treatment requirements for distillery effluents considered. Real distillery waste was introduced into the cathode to reduce ionic copper concentrations. This waste was then recirculated to the anode as a feed stock after the copper depletion step, in order to test the bioenergy self-sustainability of the system. Approx. 60-95% copper was recovered in the form of deposits depending on starting concentration. However, the recovery was low when the anode was supplied with copper depleted distillery waste. Through process control (MPPT or 0.5 V applied voltage) the amount and form of the copper recovered could be manipulated.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available