4.7 Article

Thermal stability and oil absorption of aluminum hydroxide treated by dry modification with different modifiers

Journal

Publisher

ELSEVIER
DOI: 10.1016/S1003-6326(08)60157-0

Keywords

aluminum hydroxide; dry modification; polyacrylic acid; thermal stability; oil absorption

Funding

  1. Science and Technology Program of Hunan Province, China [06SK2011]

Ask authors/readers for more resources

The thermal stability, particle size and morphology and oil absorption of aluminum hydroxide(ATH) treated by dry modification with three different modifiers were investigated. The experimental results show that the thermal stability of ATH powder is markedly improved by dry modification technology with the following modifiers such as phosphoric acid, polyacrylic acid and the mixture of phosphoric acid and polyacrylic acid. The best effect comes from pure phosphoric acid, and the initial temperature for the loss of crystal water of ATH powder modified with pure polyacrylic acid can reach about 202 degrees C that is approximately 10 degrees C higher than that of ATH powder before modification. The phenomena of agglomeration and macro-aggregate badly exist in ATH powder modified with the modifiers containing phosphoric acid. The growth of particles and agglomerations of powders are not evident in ATH powder modified with pure polyacrylic acid. The oil absorption of ATH powder modified with the modifiers containing phosphoric acid is apparently larger than that of original ATH powder and ATH powder modified with pure polyacrylic acid. The oil absorption of the ATH powder modified with pure polyacrylic acid is slightly smaller than that of original ATH powder.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available