A new ex situ method has been developed to mimic the degradation of the polymer membranes in polymer electrolyte membrane fuel cells (PEMFCs), caused by the cross-leakage of H-2 and O-2. In this ex situ setup, it is possible to expose membranes to flows of different gases with a controlled temperature and humidity. H+-form Nafion films with and without an electrode layer (Pt) have been treated in the presence of different gases in order to simulate the anode and cathode side of a PEMFC. The changes of the chemical structure occurring during the degradation tests were primarily examined by solid-state F-19 NMR spectroscopy. For completion, liquid-state NMR studies and ion-exchange capacity measurements were performed. The molecular mobility changes of the ionomer membrane upon degradation were examined for the first time by variable-temperature F-19 NMR line-shape, T-1 and T-1 rho relaxation experiments. It was found that degradation occurs only when both H-2 and O-2 are present (condition of gas cross-leakage) and when the membrane is coated with a Pt catalyst. The chemical degradation rate is found to be highest for H-2-rich mixtures of H-2 and O-2, which corresponds to the anode under OCV conditions. It is further shown that side-chain disintegration is very important for chemical degradation, although backbone decomposition also takes place. The temperature-dependent line-width and spectral anisotropy alterations were explained by the reduction of static disorder in the Nafion membrane. From the relaxation data, there is evidence for structural annealing, which is independent of the chemical degradation. Chemical degradation is considered to reduce the chain flexibility, as expressed by smaller motional amplitudes, most probably due to chain cross-linking.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.6
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available