Regeneration of full-scale commercial honeycomb monolith catalyst (V2O5-WO3/TiO2) used in coal-fired power plant

Journal

JOURNAL OF INDUSTRIAL AND ENGINEERING CHEMISTRY
Volume 18, Issue 1, Pages 513-519

Publisher

ELSEVIER SCIENCE INC
DOI: 10.1016/j.jiec.2011.11.070

Keywords

SCR; V2O5-WO3/TiO2 catalysts; Regeneration; Washing; Acidification

Funding

  1. National Science and Technology Ministry Program of China [2008BAC32B03]

Ask authors/readers for more resources

An effective and applicable method for the regeneration of used commercial full-scale honeycomb monolith catalysts in China (V2O5-WO3/TiO2) is firstly reported. The de-ionized water and dilute sulfuric acid solution with a relatively low concentration (pH = 2) are potent reagent to regenerated the catalysts used for about 30,000 h in coal-fired power plant. All samples were systematically characterized by TEM, N-2 adsorption/desorption, EDX, FT-IR and XPS techniques. The evaluation results reveal that the activity of the used catalysts can be obviously improved after regeneration processes. Moreover, the regenerated catalysts possess superior activity under different gas hourly space velocity (GHSV), and SO2 oxidation rate is lower than 1% in all cases. The regeneration method can remove the deposits, restore active sites and prevent nanoparticles aggregation as well as active phases leaching. Overall, these processes have promised as effective approaches for industrial V2O5-WO3/TiO2 catalysts regeneration. (C) 2011 The Korean Society of Industrial and Engineering Chemistry. Published by Elsevier B.V. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available