This study tested tensile bond strength (TBS) between veneering resins and polyetheretherketone (PEEK) after pre-treatment with adhesive systems. Five-hundred-seventy-six PEEK disks were fabricated, air-abraded and divided into six pre-treatment groups (n=96/group): Z-Prime Plus, Ambarino P60, Monobond Plus, Visio.link, Signum PEEK Bond, and control group without pre-treatment. Each group was divided into three subgroups of different veneering resins (n=32): Sinfony, GC Gradia and VITA VM LC. After specimen preparation with a bond area of 6.6 mm(2), half of each subgroup (n=16) was tested initially, and the other half was thermo-cycled. TBS measurements were analysed by three-way and one-way ANOVA, t-test and Weibull statistics. Groups without pre-treatment and groups pre-treated by Z-Prime Plus and Ambarino P60 showed no TBS. Pre-treatment with Monobond Plus increased the TBS values. The highest TBS before and after thermo-cycling between PEEK and all tested veneering resins was observed for groups pre-treated with Visio.link and Signum PEEK Bond.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.2
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据