The corrosion behaviour of one prominent bulk amorphous steel (BAS) alloy, (Fe44.3Cr5Co5Mo12.8Mn11.2 C-15.B-8(5.9))(98.5)Y-1.5, is compared to that of its crystalline counterpart and of the conventional steel X210Cr12. In acidic solutions, due to its single-phase nature, the BAS exhibits a much higher stability than the multiphase crystalline counterpart and the conventional steel. With increasing pH value, the overall elemental composition plays a more important role and the reactive elements Mo, Mn and Co, are assumed to be responsible for the observed lower stability of the BAS and its crystalline counterpart as compared to the conventional steel. (C) 2009 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据