4.1 Article

Cathode catalysts degradation mechanism from liquid electrolyte to membrane electrode assembly

期刊

COMPTES RENDUS CHIMIE
卷 17, 期 7-8, 页码 752-759

出版社

ELSEVIER FRANCE-EDITIONS SCIENTIFIQUES MEDICALES ELSEVIER
DOI: 10.1016/j.crci.2013.09.008

关键词

Carbon-supported platinum catalysts; Membrane electrode assembly; Half-cell durability tests; Single-cell durability tests; Potential cycling; Polymer Electrolyte Fuel Cell

向作者/读者索取更多资源

Single-cell and half-cell degradation test procedures were evaluated for carbon-supported Pt/C, PtCo/C and PtNi/C catalysts. Half-cell analyses were employed to understand the effect of the number of cycles and of the scan rate over the cathode catalysts degradation under potential cycling from 0.6 to 1.2 V. The data suggested a time-dependent degradation for all three catalytic systems. Single-cell measurements were used to evaluate the impact of catalyst degradation on fuel cell performance. The measurements in both setups showed similar ECSA and ORR mass activity losses. Specific degradation mechanisms related to Pt dissolution, Pt agglomeration, and transitional metal leaching were quantified and correlated with performance losses. (C) 2014 Published by Elsevier Masson SAS on behalf of Academie des sciences.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.1
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据