期刊
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING
卷 41, 期 11, 页码 1587-1596出版社
ELSEVIER SCI LTD
DOI: 10.1016/j.compositesa.2010.07.007
关键词
Mechanical properties; Hardness
Natural silk fiber (20%) reinforced polypropylene (PP) composites were prepared by compression molding. Tensile strength, tensile modulus, bending strength, bending modulus, impact strength and hardness of the prepared composite were found 54.7 MPa, 1826.2 MPa, 58.3 MPa, 3750.7 MPa, 17.6 kJ/m(2) and 95 shore A, respectively. To improve the biodegradable character of the composite, natural rubber (NR) was blended (10%, 25%, 50% by weight) with PP. It was found that the mechanical properties of the composite decrease with increasing NR in PP (except IS which increased rather decreasing). Environmental effect on the composite and degradation in various media were investigated in this study. Gamma radiation was used to increase the mechanical properties of the prepared composites. Increase in TS and BS were maximum at 250 krad dose for silk fiber/PP, silk fiber/PP:NR (90:10), silk fiber/PP:NR (75:25) and silk fiber/PP:NR (50:50) composites. (C) 2010 Elsevier Ltd. All rights reserved.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据