Hyaluronic acid (HYH) films were prepared from aqueous sodium hyaluronate (HYNa) solutions by anodic electrodeposition. The film thickness was varied in the range of 0-20 mu m by the variation of the deposition time and HYNa concentration. The deposition rate was low at HYNa concentration below 1 g L-1 and increased significantly in the range of 3-5 g L-1. The addition of bovine serum albumin (BSA) to the HYNa solutions resulted in increased deposition yield, which was attributed to the formation of composite HYH-BSA films. The thickness of the HYH-BSA films deposited by anodic electrodeposition was varied in the range of 0-80 mu m. The HYH and composite HYH-BSA films were studied by scanning electron microscopy, thermogravimetric analysis, differential thermal analysis, Fourier transform infrared spectroscopy and circular dichroism spectroscopy. The deposition mechanism and kinetics of deposition are discussed. (C) 2010 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据