Calcination; Porosity; Mechanical properties; Thermal properties; Chemically bonded ceramics; Energy savings
The kaolin-phosphoric acid mixtures with various percentages of phosphoric acid (5 wt%; 10 wt% and 15 wt%) have been investigated at room temperature. During the maturation and the sintering processes, acid reacts with aluminium of kaolin to give a new phase of aluminophosphate. This new phase's appearance has been confirmed by the thermal analysis, infrared spectroscopy, X-ray diffraction and scanning electron microscopy measurements before and after the sintering processes at different temperatures (800 degrees C, 1100 degrees C and 1250 degrees C). The rupture strength of the body-shaped samples made with the kaolin phosphoric acid mixtures is higher than that of those made with only kaolin. The porosity decreases with both the sintering temperature rise and the addition of phosphoric acid in the mixture. The addition of 10 wt% of phosphoric acid to the kaolin decreases its calcined temperature by 200 degrees C. (C) 2011 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据