4.7 Article

Optimizing calcination temperature of Fe/activated carbon catalysts for CWPO

期刊

CATALYSIS TODAY
卷 143, 期 3-4, 页码 341-346

出版社

ELSEVIER SCIENCE BV
DOI: 10.1016/j.cattod.2009.01.032

关键词

Calcination temperature; Oxygen surface groups; Activated carbon; CWPO; Fe/AC

资金

  1. Spanish Plan Nacional I + D + i [CTQ2005-02284/PPQ, CTQ2007-61748/PPQ, CTM2007-60577/TECNO]
  2. CAM [S-0505/AMB/0395]

向作者/读者索取更多资源

The influence of the calcination temperature (within the temperature range 150-300 degrees C) on the chemical nature of the surface as well as on the activity of an own-made Fe/AC catalyst for catalytic wet peroxide oxidation (CWPO) has been studied. The catalyst surface was characterized by means of TG, TPD and N-2 adsorption/desorption analysis. The presence of iron promotes the oxidation of the activated carbon surface, increasing the amount of oxygen surface groups. mainly carboxylic acid, anhydride and lactone groups. On the other hand, the calcination step modifies the distribution of these groups, increasing the amount of lactone groups and reducing the pH(slurry). Within the temperature range studied, the calcination temperature does not affect to the porous structure. The changes observed in the catalyst surface led to an increase of the catalytic activity as a consequence of a higher H2O2 decomposition into OH center dot radicals, probably due to a better dispersion of the active phase. Neither oxygen surface groups by themselves nor pH(slurry) seemed to have influence on the catalytic activity. (C) 2009 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据