We investigated catalytic steam reforming of aromatic hydrocarbon using toluene as a model compound. Ni/La0.7Sr0.3AlO3-delta catalyst showed high catalytic activity and low coke formation. Although the lattice oxygen in a perovskite-type support plays an important role for oxidizing CHx and coke precursor, the role of interaction between Ni and the support has not been clarified. In this study, Ni/La0.7Sr0.3AlO3-delta catalyst calcined at various temperatures (1073, 1173, 1273 and 1373 K) was prepared and used to elucidate the effect of Ni particle size on the lattice oxygen mobility. The Ni particle size increased concomitantly with increased calcination temperature, and the C-1 yield decreased from 72.9 to 15.5%. Enhancement of lattice oxygen mobility by the decrease of Ni particle size was observed by transient response tests using (H2O)-O-18 over Ni/La0.7Sr0.3AlO3-delta calcined at various temperatures. The interface between Ni and perovskite support played an important role for oxidizing coke precursor by lattice oxygen. (C) 2013 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据