Si3N4 fibers prepared from polycarbosliane are exposed in dry and wet air respectively from 800 to 1300 degrees C for up to 1 h. After dry air oxidation, an uniform SiO2 coating doped with nitrogen is formed on fiber surface. However, the coating obtained in wet air is much thicker with more complex microstructure containing sub layers of N-doped SiO2, near stoichiometric Si3N4 and graphite-like nanoribbons. Activation energy for oxidation in wet and dry air is determined as 108 and 152 kJ mol(-1), respectively. Both of the values are lower than the known Si3N4 materials with E-a of 259-485 kJ mol(-1).

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据