The effects of a SrFe12O19 addition on the hydrogen storage properties of LiAlH4 were investigated for the first time, to the best of our knowledge. The addition of the SrFe12O19 show improved dehydrogenation performance compared with that of undoped LiAlH4. In fact, the onset desorption temperatures decreased from 140 degrees C to 80 degrees C in the first reaction stage and from 180 degrees C to 135 degrees C in the second reaction stage. In terms of the dehydrogenation kinetics, the 10 wt% SrFe12O19-added LiAlH4 sample released approximately 5.54 wt% hydrogen at 130 degrees C after 20 min desorption, whereas the as-milled LiAlH4 sample released less than 0.3 wt% hydrogen in the same period of time and temperature. Kissinger analysis indicates that the apparent activation energies of the first two dehydrogenation reactions of LiAlH4 are decreased by approximately 27 and 15 kJ/mol, respectively, after the addition of SrFe12O19. It is reasonable to conclude that the formation of an in situ active species of Fe and LiFeO2 and amorphous Sr or Sr-containing phases could play a catalytic role in enhancing the dehydrogenation performance of LiAlH4. (C) 2017 Hydrogen Energy Publications LLC. Published by. Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据