This work aimed at preparing supertough PA6 blends with only a small :amount of elastomer. The PA6/SEBS-g-MA/PP blends were obtained by melt extrusion, in which the core-shell particles (PP as: core and SEBS-g-MA as shell) could be formed in situ in PA6 matrix. The morphology PA6 blends was, explained by both the thermodynamic factor (interfacial tension and spreading coefficient) and the kinetic factor (viscosity ratio). By adjusting the loading of PP and SEBS-g-MA, the core-shell particles with suitable size could be obtained, and the notched impact strength of the PA6 blends could be significantly improved. The effects of the loading of PP and SEBS-g-MA on tensile properties were also studied. Consequently, PA6 blends with high tensile strength and excellent impact strength could be obtained by loading only a small amount of SEBS-g-MA.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据