Accelerated weathering studies on the bioplastic, poly(3-hydroxybutyrate-co-3-hydroxyvalerate)

期刊

POLYMER DEGRADATION AND STABILITY
卷 126, 期 -, 页码 93-100

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.polymdegradstab.2016.01.023

关键词

PHBV; Bioplastic; Accelerated weathering; Photodegradation; Thermophysical property

资金

  1. USDA Forest Products Laboratory [08-JV-111111]

向作者/读者索取更多资源

The effect of accelerated weathering exposure time on the bioplastic, poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV) was studied. The chemical structure and thermophysical property changes of solvent cast PHBV films were examined by a combination of optical microscopy, size exclusion chromatography, FTIR and H-1 NMR spectroscopies, tensile testing, and differential scanning calorimetry (DSC). The exposed PHBV surfaces experienced surface crazing upon weathering. The molar mass of weathered PHBV was shown to decrease due to chain scission which was dominant over the crosslinking reaction mechanism, and compositional analysis showed the polymer degradation was non-random between the hydroxybutyrate-hydroxyvalerate units. The degree of crystallinity for PHBV was shown to increase significantly (by about 20%) upon weathering. Tensile tests showed that the weathered PHBV exhibited reduced ultimate strength and elongation to break, while the Young's modulus increased ascribing to an increase in crystallinity. Different degradation mechanisms (Norrish radical initiation, crosslinking, and hydrolysis) of PHBV are proposed and confirmed based on the experimental findings. This study provides degradation insight for PHBV exposed to both UV radiation and moisture. (C) 2016 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据