La2O3 modified 0.4(Ba0.8Ca0.2)TiO3–0.6Bi(Mg0.5Ti0.5)O3 ceramics for high-temperature capacitor applications

标题
La2O3 modified 0.4(Ba0.8Ca0.2)TiO3–0.6Bi(Mg0.5Ti0.5)O3 ceramics for high-temperature capacitor applications
作者
关键词
Dielectrics, Relaxor, Bi(Mg, 0.5, Ti, 0.5, )O, 3, High-temperature capacitor
出版物
CERAMICS INTERNATIONAL
Volume 41, Issue 9, Pages 11057-11061
出版商
Elsevier BV
发表日期
2015-05-20
DOI
10.1016/j.ceramint.2015.05.050