4.1 Article

Dendritic segregation and arm spacing in directionally solidified CMSX-4 superalloy

期刊

出版社

TAYLOR & FRANCIS LTD
DOI: 10.1080/13640461.2016.1166726

关键词

Single-crystal superalloy; Directional solidification; Segregation; Dendrite arm spacing

资金

  1. Romanian Authority for Scientific Research [174/2010]

向作者/读者索取更多资源

Dendritic segregation of directionally solidified columnar and single-crystal CMSX-4 was investigated. The partition coefficients derived from EDS measurements on as-cast samples in both transversal and longitudinal sections have shown strong segregation tendency of elements either to dendrite cores (Re, W) or to the interdendritic regions (Al, Ti, Ta). The dendritic segregation as a function of various secondary dendrite arm spacings (SDAS) has highlighted that Ti segregation is more sensitive to the SDAS than that of the other elements. It was also found that Cr has a tendency to accumulate at the coarse gamma prime-matrix interface. The solidification partition coefficients calculated with Pandat and the PanNi thermodynamic database showed a good agreement with the experimental data. Pandat calculations using the local chemical composition of segregated areas were also used for the optimisation of the solutioning heat treatment window. Primary ((1)) and secondary ((2)) arm spacings as important parameters that influence the dendritic segregation were measured for single-crystal rods at different distances from the cooling plate. Fitting equations were established for the experimental (1) and (2) as a function of cooling rate, the V(-0.25)G(-0.5) product and the local solidification time. Analytical calculations of the dendrite arm spacing compared with the experiments and ProCAST calculation showed good agreement.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.1
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据