4.7 Review

Stress intensity factors of various size single edge-cracked tension specimens: A review and new solutions

期刊

ENGINEERING FRACTURE MECHANICS
卷 153, 期 -, 页码 25-34

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.engfracmech.2015.12.022

关键词

Fatigue crack growth; Fracture mechanics; Stress intensity factor; Finite element analysis

资金

  1. US Air Force Academy [FA7000-11-2-0011]

向作者/读者索取更多资源

Non-dimensional geometric correction factor, beta, data for stress intensity factor, K, calculations are generated through finite element analyses and collected from the literature for axially loaded single-edge cracked plates with rotationally free and constrained loaded edges typically used in fatigue crack growth experiments. The solutions are valid for crack length-to-width ratio, alpha/W, in the range of 0.01 <= alpha/W <= 0.975 and plate height-to-width ratio, H/W, in the range of 0.8 <= H/W <= 10.0. Comparisons are made between the literature reported data and the present effort's results with generally satisfactory correlation. However, differences as large as 12.7% exist for short cracks in small H/W valued plates. (C) 2016 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据