Structure and ionic conductivity of Na3+Sc2Si P3-O12 (x=0.0, 0.2, 0.4, 0.8) NASICON materials: A combined neutron diffraction, MAS NMR and impedance study

标题
Structure and ionic conductivity of Na3+Sc2Si P3-O12 (x=0.0, 0.2, 0.4, 0.8) NASICON materials: A combined neutron diffraction, MAS NMR and impedance study
作者
关键词
NASICON, Neutron diffraction, MAS NMR, Ionic conductivity, Sodium batteries
出版物
SOLID STATE SCIENCES
Volume 111, Issue -, Pages 106470
出版商
Elsevier BV
发表日期
2020-12-13
DOI
10.1016/j.solidstatesciences.2020.106470