Laboratory investigation of rutting and fatigue in glassphalt containing waste plastic bottles

标题
Laboratory investigation of rutting and fatigue in glassphalt containing waste plastic bottles
作者
关键词
HDPE (High Density Polyethylene), Dynamic properties of asphalt, Waste materials, Recycled glass, Environment