High-translucency restorative materials are commonly used in the restoration of anterior teeth where aesthetics is a critical factor. In this in vitro study, the impact of mouthwash on the colour stability and surface characteristics of high-translucency computer-aided design and computer-aided manufacturing (CAD-CAM) dental restorative materials was evaluated. Two-hundred specimens were fabricated from five high-translucency CAD-CAM materials: a resin nano ceramic; a polymer-infiltrated ceramic network; a feldspathic ceramic; a lithium disilicate glass ceramic; and high-translucency zirconia. Each group of ceramic specimens was then divided into four subgroups: conventional mouthwash (LISTERINE); whitening mouthwash (LISTERINE Healthy White); chlorhexidine gluconate; and distilled water. Oral rinsing was simulated at 100 rpm for 180 h, representing 15 yr of clinical simulation. The specimens were then evaluated for colour, translucency, gloss, roughness, and surface morphology. Two-way ANOVA and linear mixed models were used for intergroup comparisons (alpha = 0.05). The polymer-infiltrated ceramic network and feldspathic ceramic became brighter, more opaque, less glossy, and rougher after rinsing with the whitening mouthwash. The long-term use of specific mouthwashes can cause deterioration of the optical and surface properties of high-translucency CAD-CAM dental restorations.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.1
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据