期刊
SEPARATION SCIENCE AND TECHNOLOGY
卷 55, 期 18, 页码 3427-3437出版社
TAYLOR & FRANCIS INC
DOI: 10.1080/01496395.2019.1677715
关键词
Refractory iron ore; suspension magnetization roasting; selective reduction; magnetic transformation; magnetic separation
资金
- National Natural Science Foundation of China [51904058, 51674064, 51734005, 51874105]
A process of suspension magnetization roasting and magnetic separation, which is used to separate and recover iron from fine limonite, was investigated. Iron concentrates grade of 58.29 wt.% and recovery of 91.45 wt.% were obtained under conditions of roasting time of 20 min at 560?C, CO concentration of 30%, grinding fineness of 85 wt.% passing 38 ?m and total gas volume of 500 ml/min. X-ray diffraction (XRD), vibration sample magnetometer (VSM), scanning electron microscope (SEM) revealed fine weak magnetic limonite was selectively transformed into strong magnetic magnetite, porous structure of iron ore caused by magnetization roasting was helpful for grinding and magnetic separation.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据