Hot corrosion behavior of Ni based Inconel 617 and Inconel 738 superalloys

期刊

APPLIED SURFACE SCIENCE
卷 378, 期 -, 页码 224-230

出版社

ELSEVIER
DOI: 10.1016/j.apsusc.2016.03.181

关键词

Ni-super alloys; Hot corrosion; Oxidation

向作者/读者索取更多资源

Superalloys are extensively used at high temperature applications due to their good oxidation and corrosion resistance properties in addition to their high stability were made at high temperature. Experimental measurements of hot corrosion at high temperature of Inconel 617 and Inconel 738 superalloys. The experiments were carried out at temperatures 700 degrees C, 800 degrees C and 900 degrees C for different exposure times to up to 100 h. The corrosive media was NaCl and Na2SO4 sprayed on the specimens. Seven different specimens were used at each temperature. The corrosion process is endothermic and the spontaneity increased by increasing temperature. The activation energy was found to be Ea = 23.54 and E-a = 25.18 Kj/mol for Inconel 738 and Inconel 617 respectively. X-ray diffraction technique (XRD) was used to analyze the formed scale. The morphology of the specimen and scale were examined by scanning electron microscopy (SEM). The results show that the major corrosion products formed were NiCr2O4, and Co Cr2O4 spinles, in addition to Cr2O3. (C) 2016 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据