期刊
MATERIALS & DESIGN
卷 85, 期 -, 页码 156-161出版社
ELSEVIER SCI LTD
DOI: 10.1016/j.matdes.2015.06.152
关键词
Welding spatter; Underwater wet welding; X-ray imaging system; FCAW
资金
- State Key Development Program for Basic Research of China [2013CB035502]
- State Key Lab of Advanced Welding & Joining, Harbin Institute of Technology [AWJ-M13-12]
- Shandong Provincial Science and Technology Development Project [2014GGX103033]
- China Postdoctoral Science Foundation [2014 M561343]
The spatter forming mechanism of underwater flux-cored wire wet welding is characterized by using a self-developed X-ray transmission system. Three representative spatter modes, droplet repelled spatter, explosive spatter and molten pool shock spatter, forming during underwater wet welding have been observed. The generation of droplet repelled spatter is due to the excessive repulsive forces for metal transfer. The diameter of this type of spatter is largest relatively, which can reach about 4.5 mm. In addition, explosive spatter, with size about 2.5 mm, is changed from the droplet with high horizontal speed caused by a slight explosion occurs at the touching location of the droplet and molten surface. Moreover, the dimension of molten pool shock spatter is smallest potentially among the spatter types during underwater wet welding, and it is only about 0.8 mm. It is generated from ridgy liquid column on [he molten pool surface because of the relatively severe concussion of the molten pool. The size, macroscopic pattern as well as chemical composition of these three types of spatters are different. (C) 2015 Elsevier Ltd. All rights reserved
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据