Effect of Sc and Zr on microstructures and mechanical properties of as-cast Al-Mg-Si-Mn alloys

期刊

出版社

ELSEVIER
DOI: 10.1016/S1003-6326(08)60309-X

关键词

Al-Mg alloy; Sc; Zr; microstructure; mechanical properties

向作者/读者索取更多资源

Microstructures of as-cast Al-Mg-Si-Mn alloys with and without Sc and Zr were investigated by optical microscopy, scanning electronic microscopy(SEM) and energy dispersion spectrum analysis. Addition of 0.2%-0.4% Sc can refine the grain size and change the growth morphology from dendritic to fine equi-axial crystal. The higher the addition of Sc, the finer the as-cast grain size. The tensile strength is increased by more than 30% with 0.4% Sc. Moreover, an addition of 0.1%-0.2% Zr is able to refine grain size and change the growth morphology from dendritic to equi-axial grain too, but less effective. However, Zr is found to increase the ductility of the cast alloys, and the elongation is increased to 11.97% with 0.2% Zr.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据