Initial oxidation of polycrystalline permalloy surface

期刊

SURFACE SCIENCE
卷 602, 期 17, 页码 2901-2906

出版社

ELSEVIER SCIENCE BV
DOI: 10.1016/j.susc.2008.07.012

关键词

photoelectron spectroscopy; work function measurements; adsorption kinetics; oxidation; nickel oxides; iron oxide; permalloy

资金

  1. Pluriformation program (PPF)
  2. Conseil General du Finistere
  3. Region Bretagne

向作者/读者索取更多资源

X-ray photoelectron spectroscopy (XPS) and work-function measurements were used in combination to investigate the initial steps of Permalloy (Ni80Fe20) oxidation at room temperature. They showed that, after oxygen saturation, the surface is covered by nickel oxide (NiO), nickel hydroxide (Ni(OH)(2)) and iron oxides (FexOy), and there is no preferential oxidation. Iron oxidation proceeds through the formation of FeO (Fe2+) followed with Fe2O3 growth (Fe3+). The oxidation is governed by a dissociative Langmuir-type oxidation: the sticking coefficient is decreasing over oxygen exposure. Oxidation continues by oxygen dissolution into the first layers to form a nano-oxide of about 8 angstrom in thickness. (C) 2008 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.4
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据