期刊
SOLID STATE IONICS
卷 216, 期 -, 页码 19-24出版社
ELSEVIER
DOI: 10.1016/j.ssi.2011.11.003
关键词
La6WO12; Solid oxide fuel cells; Proton conductivity; Compatibility; Cathode
Mixed ionic and electronic conductors (MIEC) such as LSM (La0.7Sr0.3MnO3-delta), LSCM (La0.7Sr0.25Cr0.5Mn0.5O3-delta) and BSCF (Ba0.5Sr0.5Co0.8Fe0.2O3-delta) have been investigated as potential cathode materials with La6WO12 (LWO) proton conducting electrolyte for use in protonic ceramic fuel cells (PCFC). Different cathode - LWO powder mixtures have been subjected to high temperature treatment (1150 degrees C during 144 h in air) and studied by X-ray powder diffraction (XRPD) and scanning electron microscopy (SEM). The analysis of the results reveals that LWO is chemically and mechanically stable with LSM and LSCM but reacts with BSCF. Symmetrical cells cathode/LWO/cathode have been studied by electrochemical impedance spectroscopy (EIS). The minimum of area specific resistance (ASR) values have been found for LSM cathode (in humidified air at 750 degrees C: ASR(LSM) = 4.3 Omega.cm(2); ASR(LSCM) = 15.5 Omega.cm(2); ASR(BSCF) = 9.7 Omega.cm(2)). Composite cathodes using a two-phase ceramic/ceramic (cer-cer) approach were also studied. In the case of LSM/LWO cathode cer-cer, it allows a significant decrease of the ASR value. (C) 2011 Elsevier B.V. All rights reserved.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据