4.7 Article

Synthesis of transversely isotropic nanoporous platinum

期刊

SCRIPTA MATERIALIA
卷 66, 期 8, 页码 503-506

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.scriptamat.2011.09.026

关键词

Nanoporous; Metal; Foam; Amorphous; Corrosion

资金

  1. Center for Integrated Nanotechnologies, a U.S. Department of Energy, Office of Basic Energy Sciences user facility at Los Alamos National Laboratory [AC52-06NA25396]
  2. Sandia National Laboratories [DE-AC04-94AL85000]

向作者/读者索取更多资源

We examine the influence of electrochemical parameters on transversely isotropic nanoporous (NP) platinum foam synthesized from amorphous PtxSi1 - (x) by dealloying. The externally applied potential controls the size of the Voronoi polyhedra on the free surface with sizes ranging from 0.01-0.35 mu m(2). The shape of the amperometric curve is governed by the dealloying front progression that in turn advances faster than the rate of diffusion of Si in the electrolyte. (C) 2011 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据