The Comparison Effect of Sorbitol and Glycerol as Plasticizing Agents on the Properties of Biodegradable Polyvinyl Alcohol/Rambutan Skin Waste Flour Blends

期刊

POLYMER-PLASTICS TECHNOLOGY AND ENGINEERING
卷 51, 期 4, 页码 432-437

出版社

TAYLOR & FRANCIS INC
DOI: 10.1080/03602559.2011.639827

关键词

Glycerol; Plasticizing agent; Polyvinyl alcohol; Rambutan skin waste flour; Sorbitol

资金

  1. USM
  2. Research University grant [1001/PBAHAN/814065]

向作者/读者索取更多资源

The comparison effect of glycerol and soritol as plasticizing agents on properties of biodegradable polyvinyl alcohol (PVOH)/rambutan skin waste flour (RWF) films were studied. Results showed that the glycerol-plasticized films exhibited higher elongation at break, but lower tensile strength and Young's modulus than sorbitol-plasticized films. Water vapor transmission rate (WVTR) was increased with the addition of plasticizing agents. The glycerol-plasticized films showed higher WVTR which indicated that glycerol had more positive contribution to water affinity compared to sorbitol. Biodegradability test revealed that the weight loss of unplasticized PVOH/RWF films was lower than glycerol-and sorbitol-plasticized PVOH/RWF films.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

3.9
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据