Material valorisation of amorphous polylactide. Influence of thermo-mechanical degradation on the morphology, segmental dynamics, thermal and mechanical performance

期刊

POLYMER DEGRADATION AND STABILITY
卷 97, 期 4, 页码 670-678

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.polymdegradstab.2011.12.019

关键词

Polylactide (PLA); Material valorisation; Mechanical recycling; Thermo-mechanical degradation; Cold-crystallization; Segmental dynamics

资金

  1. Spanish Ministry of Science and Innovation [UPOVCE-3E-013]
  2. Spanish Ministry for Education
  3. Generalitat Valenciana [ACOMP/2011/189]
  4. Universitat Politecnica de Valencia (UPV, Spain) [PAID 05-09-4331]
  5. Royal institute of Technology (KTH, Sweden)

向作者/读者索取更多资源

This paper reports the effects of multiple mechanical recycling on the structure and properties of amorphous polylactide (PIA). The influence of the thermo-mechanical degradation induced by means of five successive injection cycles was initially addressed in terms of macroscopic mechanical properties and surface modification. A deeper inspection on the structure and morphology of PLA was associated to the thermal properties and viscoelastic behaviour. Although FT-IR analysis did not show significant changes in functional groups, a remarkable reduction in molar mass was found by viscometry. PIA remained amorphous throughout the reprocessing cycles, but the occurrence of a cold-crystallization during DSC and DMTA measurements, which enthalpy increased with each reprocessing step, suggested chain scission due to thermo-mechanical degradation. The effect of chain shortening on the glass-rubber relaxation studied by DMTA showed an increase in free volume affecting the segmental dynamics of PLA, particularly after the application of the second reprocessing step, in connection to the overall loss of performance showed by the remaining properties. (C) 2012 Elsevier Ltd. All rights reserved.