期刊
POLYMER DEGRADATION AND STABILITY
卷 94, 期 3, 页码 355-364出版社
ELSEVIER SCI LTD
DOI: 10.1016/j.polymdegradstab.2008.12.004
关键词
Polyester; Nanocomposites; Thermal decomposition; Halogen-free; Flame retardancy; FTIR
资金
- Deutsche Forschungsgemeinschaft (DFG) [SCHA 730/6-1, Po 575/8-1]
- IPF
This paper deals with the thermal decomposition behaviour of a new fire retardant 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide (DOPO)-containing aliphatic-aromatic polyester and its nano-composites with natural layered silicate (montmorillonite) under inert atmosphere studied by TGA-FTIR, Pyrolysis-GC/MS of volatile products and ATR-FTIR of non-volatile decomposition products. The phosphorus-containing polyester undergoes decomposition in two steps between 340 and 516 degrees C. The first step is associated with the release of carbon dioxide, acetaldehyde, ethene, acid-containing products (mainly benzoic acid) resulting in the formation of polyarylates followed by their decomposition in the second step with the evolution of carbon dioxide. DOPO-containing products, esters (mainly diethenyl terephthalate), carbon monoxide, acids and water are released through both stages. At the end of decomposition polyaromatic structures, diarylketones and organophosphorus esters built into the chemical structure of the char develop in the solid residue. The modification of the polyester with a layered silicate does not change the composition of the pyrolysis products, only their yield, and tended to diminish the charring of the polymer. A thermal decomposition scheme of the P-polyester is proposed and the mass spectra of some DOPO-containing products are discussed. (C) 2008 Elsevier Ltd. All rights reserved.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据