4.7 Article

The second virial coefficients of highly-purified ring polystyrenes in cyclohexane

期刊

POLYMER
卷 50, 期 5, 页码 1300-1303

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.polymer.2009.01.019

关键词

Ring polystyrene; Theta temperature; Topological interaction

向作者/读者索取更多资源

The second virial coefficients A(2) of ring polystyrenes with high purity in cyclohexane were measured by light scattering in the temperature range 27.0-34.5 degrees C. The purity of four samples with M-w of 16k, 42k, 110k and 570k was determined to be all over 96% by HPLC. It has been found that A(2)s of all the samples are definitely positive at the theta temperature of linear polystyrene, 34.5 degrees C, and the measured values for four samples converged to zero at 27.7 degrees C with decreasing temperature. This value is below the previously reported one, but it is quite consistent with the predicted value based on the topological repulsive interaction among the ring polymer molecules. (c) 2009 Elsevier Ltd. All rights reserved

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据