The absorption of hydrogen in thin V(001) films under pressures of 1-10(5) Pa H-2 and at temperatures between 350 and 530 K was studied as a function of film thickness between 50 and 5 nm using in situ electrical resistivity measurements. The critical temperatures for the order-disorder transitions taking place in the V-H system are decreased with decreasing film thickness. At 370 K, the high-concentration (epsilon-VH) phase disappears as the thickness of the film is reduced from 50 to 10 nm and the low-concentration (beta-V2H) phase follows when the film thickness is further decreased to 5 nm. The difference in solubility at 530 K of H in the alpha phase of V films down to 10 nm is small but it increases for lower temperatures. At low concentrations the heat of solution in the 10 nm film is somewhat lower than in the bulk, but around H/V = 0.07, the values of Delta H-H in the film approach those of the bulk. The values of Delta S-H(nc) of the film are rather close to those of the bulk. Significant difference is found in the pressure-resistivity isotherms above the maximum of the residual resistivity, Delta R-max. For the 10 nm film, in contrast to the 50 nm film, a minimum is located just beyond Delta R-max for the whole temperature range but the difference between the maximum and minimum starts to decrease above 420 K. This results in, by extrapolation, the vanishing of the maximum around 520 K. We suggest that this phenomenon is the result of an Oz -> T transition due to a final size effect. This transition means additional randomly distributed interstitial sites available for the H atoms in the lattice of the V film leading to a continuous increase in the residual resistivity with H concentration.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据