4.3 Article

Perforation of graphite in boiling mineral acid

期刊

PHYSICA STATUS SOLIDI B-BASIC SOLID STATE PHYSICS
卷 249, 期 12, 页码 2620-2624

出版社

WILEY-V C H VERLAG GMBH
DOI: 10.1002/pssb.201200143

关键词

acid treatment; chemical modification; electronic structure; graphite oxide; perforated graphite

资金

  1. Russian Foundation for Basic Research [12-03-00579]
  2. bilateral Program Russian-German Laboratory at BESSY

向作者/读者索取更多资源

Perforation of graphite is carried out by treating the graphite oxide with a boiling mineral acid H2SO4 or H3PO4. High-resolution transmission electron microscopy shows formation of a large number of vacancy defects (holes) in the graphene sheets, which are caused more likely by the CO2 liberation during the reduction process. The characteristic size of the holes is about 2?nm. The obtained materials are comparatively examined by X-ray diffraction, Raman and IR-absorption spectroscopy, X-ray photoelectron and near-edge X-ray absorption fine structure spectroscopy. It is found that the products obtained using a strong acid H2SO4 and a weak acid H3PO4 are different in the concentration and electronic state of oxygen and the mean distance between defects. [GRAPHICS] Left, schematic representation of the perforated graphite (PG); right, NEXAFS OK-edge spectra of the PG obtained using H3PO4 and H2SO4 acids demonstrate the different electronic state of oxygen in the samples. (C) 2012 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.3
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据