4.7 Article

Laser welding of thin foil nickel-titanium shape memory alloy

期刊

OPTICS AND LASERS IN ENGINEERING
卷 49, 期 1, 页码 121-126

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.optlaseng.2010.08.007

关键词

Shape memory alloy; NiTi; Laser welding; Taguchi method; Pitting corrosion

类别

资金

  1. Research Office of The Hong Kong Polytechnic University, Hong Kong Special Administrative Region, China [G-U405]

向作者/读者索取更多资源

In this study, two 127 Taguchi experiments were carried out to study the effect of fibre laser welding parameters and their interactions upon the weld bead aspect ratio of nickel-titanium thin foil. The optimum parameters to produce full penetrated weld with the largest aspect ratio and desirable microstructure were successfully obtained by the Taguchi experimental design. The corrosion property of the optimized NiTi weld in Hank's solution at 37.5 degrees C was studied and compared with the as-received NiTi. To improve the corrosion properties of the weld, the effect of post-weld-heat-treatments ranging from 573 to 1173 K was investigated. The corrosion properties, surface morphology, microstructure and Ti/Ni ratio of the heat-treated NiTi weld were analysed. It was found that a post-weld heat treatment at 573 K for 1 h provided the best pitting corrosion resistance at the weld zone. (C) 2010 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据