4.6 Article

Surface aspects of discolouration in Bisphenol A Polycarbonate (BPA-PC), used as lens in LED-based products

期刊

OPTICAL MATERIALS
卷 37, 期 -, 页码 155-159

出版社

ELSEVIER SCIENCE BV
DOI: 10.1016/j.optmat.2014.05.015

关键词

Bisphenol A Polycarbonate (BPA-PC); XPS; Discolouration; LED lens

资金

  1. Research Program of the Materials innovation institute M2i [M71.9.10380]

向作者/读者索取更多资源

The surface-related reactions during discolouration of Bisphenol A Polycarbonate (BPA-PC), used as LED lens plates, under thermal stress are studied. X-ray photoelectron spectroscopy (XPS) has been used to monitor the changes in the surface chemistry of BPA-PC plates over a temperature range of 100-140 degrees C for a period up to 3000 h. Increasing time under thermal stress is associated with the discolouration, and increase in the yellowing index (YI) of PC plastic lens. The XPS results show that discolouration is associated with oxidation at the surface, finding a significant increase in the signal ratio O-1s/C-1s in the XPS spectra of degraded specimens. During thermal ageing, the C H concentration decreases and new oxide features C=O and O-C=O form, with the latter being a support for oxidation at the surface being a major reaction during discolouration. Results also show that irradiation with blue light during thermal ageing accelerates the kinetics of discolouration and the increased O-1s/C-1s ratio in XPS spectra. (C) 2014 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据