Inconel 718 (2 mm thick) was welded using argon and helium gas shielded tungsten arc welding process with a filler metal. Both constant current and compound current pulse modes were applied and the cooling rates calculated. The dependence of Laves phase formation, dendrite arm spacing and niobium segregation ratios in fusion zone on the nature of shielding gases and current was studied. The maximum instantaneous weld cooling rate was achieved for the combination of Helium shielding gas and compound current pulse mode. This ultimately resulted in reduction of laves phase, segregation of niobium and dendrite arm spacing in the fusion zone. (C) 2013 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据