Zirconium is always present in Ni base superalloys as it enhances their creep properties. In the present study, the influence of very small Zr additions, 100-400 ppm, i.e. 0.01-0.04 wt.%, on hot tearing of IN738LC superalloy is experimentally investigated using dedicated turbine blade castings. Although the Zr content remains very small, it has a strong effect on hot tearing tendency. Microstructure of hot tear in as-cast samples reveal that grain size and secondary dendrite arm spacing have no significant effect on hot tearing. On the other hand eutectic phase volume fraction and its dispersion or spreading along grain boundaries drastically affect the hot tearing propensity and strongly increase with increasing amounts of Zr. Hence grain coalescence becomes impossible at grain boundaries covered with eutectic phase films. With increasing Zr content, gain coalescence between two distinct grains with no interdendritic phase requires more undercooling. Coalescence is retarded and occurs deeper in the mush zone, i.e. at lower temperatures resulting in a higher sensitivity to hot tearing. Finally, it is shown that a reduction of Zr content to 0.02 wt.% is required to fully suppress hot tearing in polycrystalline IN738LC blades. (C) 2013 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据